Browse Standards ARP1341B
Historical REAFFIRMED 2018-08-23

Determining Decarburization and Carburization in Finished Parts of Carbon and Low-Alloy Steels ARP1341B

This document provides a recommended practice for determining decarburization and carburization in heat treated carbon and low-alloy steel parts other than case hardened parts. It is not applicable to raw materials.
ARP1341C
2024-01-22
Latest
Stabilized
ARP1341B
2018-08-23
Historical
Reaffirmed
ARP1341A
1995-05-01
Historical
Reaffirmed
ARP1341
1974-12-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 11% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Heat Treatment of Carbon and Low-Alloy Steel Parts Minimum Tensile Strength Below 220 ksi (1517 MPa)

AMS2759/1J

View Details

STANDARD

Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher

AMS2759/2K

View Details

STANDARD

Steel, Corrosion-Resistant, Investment Castings 16Cr - 1.9Ni - 0.08N As Cast

AMS5353F

View Details

Get Involved

Want to participate in updating this standard?

X