Browse Standards AMS5707E
Historical REVISED 1974-12-01

ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 58Ni Consumable Electrode or Vacuum Induction Melted 1825 - 1900° F (996.1 - 1037.8° C) Solution, Stabilization, and Precipitation Heat Treated AMS5707E

This specification covers a corrosion and heat resistant nickel alloy in the form of bars, forgings, flash welded rings, and stock for forging or flash welded rings.
AMS5707P
2023-03-23
Latest
Revised
AMS5707N
2017-06-13
Historical
Revised
AMS5707M
2015-01-14
Historical
Revised
AMS5707L
2013-12-02
Historical
Reaffirmed
AMS5707K
2007-01-09
Historical
Revised
AMS5707J
2000-08-01
Historical
Revised
AMS5707H
1994-08-01
Historical
Revised
AMS5707G
1989-01-01
Historical
Revised
AMS5707F
1981-04-01
Historical
Revised
AMS5707E
1974-12-01
Historical
Revised
AMS5707D
1973-05-01
Historical
Revised
AMS5707C
1970-05-01
Historical
Revised
AMS5707B
1966-03-01
Historical
Revised
AMS5707A
1964-01-01
Historical
Revised
AMS5707
1963-07-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 9% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.

Get Involved

Want to participate in updating this standard?

X