Historical REVISED 2018-08-17

Steel, Corrosion-Resistant, Bars, Wire, and Forgings 12Cr - 8.5Ni - 1.2Ti - 2.0Cu Vacuum Induction Plus Vacuum Consumable Electrode Melted Solution Heat Treated, Precipitation Hardenable AMS5617K

This specification covers two grades of a premium aircraft-quality, corrosion-resistant steel in the form of bars, wire, forgings, and forging stock.
AMS5617L
2024-01-22
Latest
Revised
AMS5617K
2018-08-17
Historical
Revised
AMS5617J
2012-02-09
Historical
Reaffirmed
AMS5617H
2000-09-01
Historical
Revised
AMS5617G
1994-04-01
Historical
Reaffirmed
AMS5617F
1988-07-01
Historical
Revised
AMS5617E
1981-04-01
Historical
Revised
AMS5617D
1979-01-01
Historical
Revised
AMS5617C
1977-07-01
Historical
Revised
AMS5617B
1976-01-01
Historical
Revised
AMS5617A
1973-12-01
Historical
Revised
AMS5617
1969-05-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 10% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Steel, Corrosion-Resistant, Bars, Wire, and Forgings and Forging Stock 17Cr - 0.52Mo (0.95 - 1.20C) (440C)

AMS5630M

View Details

STANDARD

Steel, Corrosion-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Rings 15Cr - 6.5Ni - 0.75Mo - 0.30 Cb (Nb) - 1.5Cu Consumable Electrode Remelted, Solution Heat Treated Precipitation Hardenable

AMS5773F

View Details

STANDARD

Steel, Corrosion and Heat-Resistant, Sheet, Strip, and Plate 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V 1800 °F (982 °C) Solution Heat Treated

AMS5525L

View Details

Get Involved

Want to participate in updating this standard?

X