Aluminum Alloy, Sheet and Plate 4.4Cu - 1.5Mg - 0.60Mn (2024-0) Annealed; or when specified, “As Fabricated” (2024-F) AMS4035L

This specification covers an aluminum alloy in the form of sheet and plate supplied in the annealed (O) condition. When specified, product shall be supplied in the “as fabricated” (F) temper.
AMS4035M
2017-12-07
Latest
Revised
AMS4035L
2011-12-19
Historical
Revised
AMS4035H
2011-08-09
Historical
Reaffirmed
AMS4035K
2008-05-01
Historical
Reaffirmed
AMS4035J
1996-09-01
Historical
Revised
AMS4035G
1979-10-01
Historical
Revised
AMS4035F
1968-05-01
Historical
Revised
AMS4035E
1964-06-01
Historical
Revised
AMS4035D
1955-08-01
Historical
Revised
AMS4035C
1952-06-01
Historical
Revised
AMS4035B
1946-04-01
Historical
Revised
AMS4035A
1942-08-01
Historical
Revised
AMS4035
1940-06-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 9% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Aluminum Alloy, Sheet and Plate 1.0Mg - 0.60Si - 0.28Cu - 0.20Cr (6061; -T4 Sheet, -T451 Plate) Solution Heat Treated and Naturally Aged

AMS4026M

View Details

STANDARD

Aluminum Alloy, Sheet and Plate 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr Annealed (7075-O) or when specified, “As Fabricated” (7075-F)

AMS4044N

View Details

STANDARD

Aluminum Alloy, Alclad Sheet and Plate 6.3Cu - 0.30Mn - 0.18Zr - 0.10V - 0.06Ti Alclad 2219-T31; Sheet, Solution Heat Treated and Cold Worked Alclad 2219-T351; Plate, Solution Heat Treated and Stress Relieved

AMS4095E

View Details

Get Involved

Want to participate in updating this standard?

X