Browse Standards AMS4021H
Current STABILIZED 2017-05-30

Aluminum Alloy, Alclad Sheet and Plate, 1.0Mg - 0.60Si - 0.28Cu - 0.20Cr (Alclad 6061-0) Annealed(STABILIZED May 2017) AMS4021H

This specification covers an alclad aluminum alloy in the form of sheet and plate.
AMS4021H
2017-05-30
Latest
Stabilized
AMS4021G
2012-03-29
Historical
Reaffirmed
AMS4021F
1993-10-01
Historical
Revised
AMS4021E
1992-04-01
Historical
Reaffirmed
AMS4021D
1977-01-15
Historical
Revised
AMS4021C
1968-11-01
Historical
Revised
AMS4021B
1958-08-15
Historical
Revised
AMS4021A
1953-02-15
Historical
Revised
AMS4021
1951-10-01
Historical
Issued

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 10% off list price.
Login to see discount.
Special Offer: AeroPaks offers a customized subscription plan that is cost-effective and allows you to choose the number of downloads and Aerospace and Aerospace Material documents you need. Find more information here.
We also recommend:
STANDARD

Aluminum Alloy, Sheet 2.4Li - 1.3Cu - 0.95Mg - 0.10Zr (8090-T6) Solution and Precipitation Heat Treated (Unrecrystallized)

AMS4259B

View Details

STANDARD

Aluminum Alloy, Rolled or Cold Finished Bars, Rods, and Wire 5.6Zn - 2.5Mg - 1.6Cu - 0.23Cr (7075-T73, T7351) Solution Heat Treated, Stress Relieved by Stretching, and Overaged

AMS4124F

View Details

STANDARD

Aluminum Alloy Tubing, Seamless, Drawn 1.8Cu - 1.0Mg - 0.8Si - 0.20Cr Solution Heat Treated, Stress-Relieved by Stretching, and Aged (2013-T4511)

AMS4469A

View Details

Get Involved

Want to participate in updating this standard?

X