An Investigation of the Effect of Post Forging Cooling Rate on the Microstructure and Properties of Microalloyed Steels 930961

Medium carbon steels have been traditionally used for high strength forging applications. These steels contain several alloying elements like chromium, nickel and molybdenum which enable them to attain excellent hardenability and toughness upon heat treatment (quenching and tempering). Microalloyed (MA) medium carbon forging steels are gaining acceptance as a replacement for the traditional quenched and tempered grades as they do not require post forging heat treatment and hence represent substantial savings in manufacturing costs. Since the chief advantage of MA steels lies in the savings of heat treatment costs, the post-forging cooling rate is one of the primary parameters for controlling microstructure and toughness of the forged part.
This paper investigates the effect of different cooling rates on the microstructure and mechanical properties of MA steels. Experiments were conducted by cooling test billets in different media. The billets were then examined microstructurally and physical testing was also performed. Regression correlations (empirical relationships) analyzing the effect of cooling rate on the microstructure and mechanical properties have also been presented.

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 16% off list price.
Login to see discount.
Special Offer: Download multiple Technical Papers each year? TechSelect is a cost-effective subscription option to select and download 12-100 full-text Technical Papers per year. Find more information here.
We also recommend:
STANDARD

Steel, Corrosion-Resistant, Bars, Wire, and Forgings 18Cr - 9.0Ni Free Machining

AMS5640V

View Details

STANDARD

Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 74Ni - 7.0Cr - 16.5Mo Solution Heat Treated

AMS5771G

View Details

STANDARD

Steel, Corrosion and Heat-Resistant, Bars and Wire 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V 1800 °F (982 °C) Solution Heat Treated and Work-Strengthened Consumable Electrode Remelted 200 ksi (1379 MPa) Tensile Strength Capability

AMS5726E

View Details

X