Preparation and Physical Properties of Two-Packaged Polyurethane Coatings for Silver Mirror Layer Protection 2009-01-0570

The gel fraction and the curing rate of the silver mirror protective film according to the curing condition were investigated. Two-packaged polyurethane dry film made from acryl polyol and three different isocyanate curing agents (HDI-biuret, HDI-trimer and IPDI trimer) were built on the silver mirror layer in order to protect the layer. FTIR/ATR spectra showed the isocyanate content was clearly decreased and the gel fraction was increased as curing temperature and time were increased. The optimum curing condition of the silver mirror protective film was 80□ and 30 minutes. The dry film prepared with the optimum condition satisfied all tests in our materials specification for automotive interior parts. Moreover, the pencil hardness of the film containing dibutyltin dilaurate was stronger than the film without catalyst.

SAE MOBILUS

Subscribers can view annotate, and download all of SAE's content. Learn More »

Access SAE MOBILUS »

Members save up to 16% off list price.
Login to see discount.
Special Offer: Download multiple Technical Papers each year? TechSelect is a cost-effective subscription option to select and download 12-100 full-text Technical Papers per year. Find more information here.
We also recommend:
TECHNICAL PAPER

Failure Mechanisms in Automotive Exhaust Decouplers

2004-01-0858

View Details

TECHNICAL PAPER

Bending Performance of Advanced High Strength Steel Tubes

2009-01-0085

View Details

TECHNICAL PAPER

Tangentially Mounted Inserts: A Good Avenue for Recycle

2009-01-0134

View Details

X