ALnalyse of System Factors Affecting Performance in Lean NOx Catalysis. 2. The Deleterious Role of Parasitic Homogeneous Hydrocarbon Oxidation on the Performance of High Temperature Lean NOx Catalysts

1998-10-19
982604
Increasing interest in lean NOx catalysis at temperatures between about 300-550°C has led to development of catalytic materials with thermal durability considerably improved over academic benchmark catalysts such as Cu-ZSM-5. The breaching of thermal durability barriers brings new obstacles into focus. Practical implementation of high temperature HC-based lean NOx catalysis entails delivery of hydrocarbons to the catalyst inlet at high temperatures. We have found initially unexpected, but scientifically precedented, phenomena regarding gas-phase kinetic instability of hydrocarbons in diesel exhaust atmospheres above 300°C. Around 300°C, homogeneous hydrocarbon oxidation can begin to occur. Rates of oxidation decrease between about 350-450°C and then increase again at higher temperatures. Some apparent NOx disappearance that does not correspond to chemical reduction of NOx can also occur homogeneously throughout this temperature range.
X