Technical Paper

Low Friction Coating for High Temperature Bolted Joints in IC Engines

2023-04-11
2023-01-0733
The IC engine still plays an important role in global markets, although electrified vehicles are highly demanded in some markets. Emission requirements for stoichiometric operation are challenging. This requires the bolted joints for turbo, EGR (Exhaust Gas Recirculation) and exhaust manifold to work under much higher temperature than before. How to avoid fastener breakage due to bolt bending caused by cyclic changes of the thermal conditions in engines is a big challenge. The temperatures of the components in the exhaust, EGR (Exhaust Gas Recirculation) and turbo systems change from ambient temperature to about 800 ~ 1000 °C when engines run at peak power with wide-open throttle. The temperature change induces catastrophic cyclic bending and axial strain to the fasteners. This research describes a method to reduce the cyclic bending displacement in the fasteners using a low friction washer.
Technical Paper

Fatigue Behaviour of Thin Electrical Steel Sheets at Room Temperature

2023-04-11
2023-01-0805
Electrical steel, also known as silicon steel, is a ferromagnetic material that is often used in electric vehicles (EVs) for stator and rotor applications. Since the design and manufacturing of rotors require the use of laminated thin electrical steel sheets, the fatigue characterization of these single sheets is of interest. In this study, a 0.27mm thick non-oriented electrical steel sheet was tested under cyclic loading in the load-controlled mode with the load ratio R = 0.1 at room temperature. The specimens were prepared using the Computer Numerical Control (CNC) machining method. The Smith-Watson-Topper mean stress correction was used to find the equivalent fully reversed stress-life (S-N) curve. The Basquin equation was used to describe the fatigue strength of the electrical steel and the fatigue parameters were extracted. Furthermore, a design curve with a reliability of 90% and a confidence level of 90% was generated using Owen’s Tolerance Limit method.
Technical Paper

Effect of Edge Finish on Fatigue Behavior of Thin Non-oriented Electrical Steel Sheets

2023-04-11
2023-01-0803
Strict environmental regulations are driving the automotive industry toward electric vehicles as they offer zero emissions. A key component in electric vehicles is the electric motor, where the stator and rotor are manufactured from stacks of thin electrical steel sheets. The electrical steel sheets can be cut in different ways, and the cutting methods may significantly affect the fatigue strength of the component. It is important to understand the effect of the cutting processes on the fatigue properties of electrical steel to ensure there is no premature failure of the electric motor resulting from an improper cutting process. This investigation compared the effect of three different edge preparation methods (stamping, CNC machining, and waterjet cutting) on the fatigue performance of 0.27mm thick electrical steel sheets. To investigate the effect of the edge finish on fatigue behavior, surface roughness was measured for these different samples.
Technical Paper

Fatigue Behavior of Stamped Electrical Steel Sheet at Room and Elevated Temperatures

2023-04-11
2023-01-0804
Electrical steels are silicon alloyed steels that possess great magnetic properties, making them the ideal material choice for the stator and rotor cores of electric motors. They are typically comprised of laminated stacks of thin electrical steel sheets. An electric motor can reach high temperatures under a heavy load, and it is important to understand the combined effect of temperature and load on the electrical steel’s performance to ensure the long life and safety of electric vehicles. This study investigated the fatigue strength and failure behavior of a 0.27mm thick electrical steel sheet, where the samples were prepared by a stamping process. Stress-control fatigue tests were performed at both room temperature and 150°C. The S-N curve indicated a decrease in the fatigue strength of the samples at the elevated temperature compared to the room temperature by 15-25 MPa in the LCF and HCF regimes, respectively.
Technical Paper

Embrittlement of SiMo Ductile Cast Iron Exhaust Manifold and Evaluation using Sehitoglu Damage Model

2022-03-29
2022-01-0280
Sehitoglu damage model is often applied to evaluate thermomechanical fatigue (TMF) performance of the components in the environment of high temperature in finite element analysis (FEA). SiMo ductile cast irons have been widely used for exhaust manifolds in propulsion systems. The manifold experiences TMF due to the limitation of thermal expansion in the assembled condition. Mechanical strain and damage are therefore introduced by the constraints. On the other hand, it is known that ductile cast iron exhibits embrittlement at the temperature around 400°C due to the addition of magnesium (Mg) in order to obtain graphite nodules. This mechanical behavior at 400°C, which has to be considered in design, makes the ductile cast irons only partially satisfy the assumptions of the Sehitoglu damage model. In the present work, a two-step approach is presented to evaluate the sensitivity of the manifold geometry to the 400°C embrittlement using the Sehitoglu model.
Technical Paper

Numerical Investigation in a Gear Drive of an Engine Balancing Unit with Respect to Noise, Friction and Durability

2015-09-06
2015-24-2526
This paper presents a methodology for numerical investigation of a full flexible balancer drive together with engine and crank train under realistic operating conditions where shaft dynamics, gear contact and rattle impacts, gear root stresses and friction losses in bearings and gear interaction are taken into account and can be balanced against each other to achieve the design criteria. Gear rattle is driven by the speed fluctuation of the crank train, the resistance torque (mainly friction), shaft inertia and the backlash in the gears. The actual trend to engine downsizing and up-torqueing increases the severity to rattle as engines are running on higher combustion pressures. This increases torque and speed fluctuation, which makes the detailed investigation in this torque transfer even more demanding. A common method to reduce gear rattle is the usage of so-called scissors gears.